X-radiography inspection techniques are generally used in non-destructive evaluation
industry. Manual assessment of the inspection may fail and turn into false assessment due
to a large number of examining while inspection process. Accordingly, incorrect
assessment through human vision may cause immense industry disaster. Therefore, it is
essential to examine through machine vision, which is capable to avoid false assessment.
Digital X-radiography has widely been used in Non-Destructive Testing (NDT) and
particularly in weld defect detection. Weld defects occurrence is an unavoidable problem
during the welding process. Most common weld defects some of which are porosity, gas
pore, tungsten inclusion, longitudinal crack, lack of penetration, and slag inclusion.
Digital image processing techniques are a foremost way to experiment in the NDT. The
detection and classification of weld defects depend on the quality of the digitized image,
which is subjected to certain factors, such as noise, the mode of the image histogram,
defects of different dimensions, indiscernible defects in the image background, and low
contrast or unevenly illuminated image. More accuracy can be achieved during classification
of weld defects are always be subject to the deliverables of low and mid-level image
processing techniques. Therefore, it is desirable to provide more importance for these levels
in the weld X-radiography image.
Les informations fournies dans la section « Synopsis » peuvent faire référence à une autre édition de ce titre.
Vendeur : GreatBookPrices, Columbia, MD, Etats-Unis
Etat : As New. Unread book in perfect condition. N° de réf. du vendeur 45075844
Quantité disponible : Plus de 20 disponibles
Vendeur : GreatBookPrices, Columbia, MD, Etats-Unis
Etat : New. N° de réf. du vendeur 45075844-n
Quantité disponible : Plus de 20 disponibles
Vendeur : Rarewaves.com USA, London, LONDO, Royaume-Uni
Paperback. Etat : New. N° de réf. du vendeur LU-9783311791706
Quantité disponible : Plus de 20 disponibles
Vendeur : PBShop.store US, Wood Dale, IL, Etats-Unis
PAP. Etat : New. New Book. Shipped from UK. THIS BOOK IS PRINTED ON DEMAND. Established seller since 2000. N° de réf. du vendeur L0-9783311791706
Quantité disponible : Plus de 20 disponibles
Vendeur : California Books, Miami, FL, Etats-Unis
Etat : New. N° de réf. du vendeur I-9783311791706
Quantité disponible : Plus de 20 disponibles
Vendeur : PBShop.store UK, Fairford, GLOS, Royaume-Uni
PAP. Etat : New. New Book. Delivered from our UK warehouse in 4 to 14 business days. THIS BOOK IS PRINTED ON DEMAND. Established seller since 2000. N° de réf. du vendeur L0-9783311791706
Quantité disponible : Plus de 20 disponibles
Vendeur : Ria Christie Collections, Uxbridge, Royaume-Uni
Etat : New. In English. N° de réf. du vendeur ria9783311791706_new
Quantité disponible : Plus de 20 disponibles
Vendeur : Majestic Books, Hounslow, Royaume-Uni
Etat : New. Print on Demand. N° de réf. du vendeur 401117648
Quantité disponible : 4 disponible(s)
Vendeur : Books Puddle, Woodside, NY, Etats-Unis
Etat : New. Print on Demand. N° de réf. du vendeur 26396307983
Quantité disponible : 4 disponible(s)
Vendeur : Biblios, Frankfurt am main, HESSE, Allemagne
Etat : New. PRINT ON DEMAND. N° de réf. du vendeur 18396307973
Quantité disponible : 4 disponible(s)